EP36AN Product Information

EP36AN One Component, B-stage Epoxy

One Component, B-Stage, High Temperature Resistant, Toughened Epoxy System for Potting, Encapsulation, Coating and Bonding Applications; Featuring Very High Thermal Conductivity and Electrical Isolation. Available in 30 Gram Cookies.

EP36AO Product Information

EP36AO One Component B-stage Epoxy

One Component, B-Stage, High Temperature Resistant, Toughened Epoxy System for Potting, Encapsulation, Coating and Bonding Applications; Featuring Thermal Conductivity and Electrical Isolation. Available in 30 Gram Cookies.

EP37-3FLFAN Product Information

EP37-3FLFAN Two Part Epoxy System

Two Component, Room Temperature Curing, Highly Thermally Conductive, Electrically Isolating Epoxy For Potting, Bonding, Sealing & Coating Featuring Flexibility and Low Viscosity.

EP37-3FLFAO Product Information

EP37-3FLFAO Two Part Epoxy

Two component epoxy compound for potting, bonding, sealing and coating

EP3ANHT Product Description

EP3ANHT One Part Epoxy

One Component Abrasion, Thermal Shock and Heat Resistant Thermally Conductive Epoxy for Electrical Potting Encapsulation and Bonding

EP3AOHT Product Description

EP3AOHT One Part Epoxy

One Component Abrasion, Thermal Shock and Heat Resistant Thermally Conductive Epoxy for Electrical Potting Encapsulation and Bonding

EP3AOHTLV Product Description

EP3AOHTLV One Component Epoxy

One Component Abrasion, Thermal Shock, and Heat Resistant Thermally Conductive Epoxy for Electrical Potting, Encapsulation and Bonding

EP3HTS Product Information

EP3HTS One Part Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.

EP3HTSMed Product Information

EP3HTSMed One Part Medical Grade Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed

EP3RR-1 Product Description

EP3RR-1 One Part Epoxy

One Part, Lower Viscosity, Thermally Conductive Epoxy System for High Performance Potting, Encapsulation and Underfill Applications Featuring Exceptional Dimensional Stability and Rapid Curing at 230-250°F.