EP36CLV One component, B-staged epoxy. Features low viscosity and excellent electrical insulation properties. Operating service temperature range -100°F to +500°F. Combines flexibility and toughness. Superior chemical resistance to water, acids, bases, fuels and oils. Elongatio >50%. |
![]() |
EP36FR Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
![]() |
EP37-3 Resilient, optically clear, two component epoxy resin system. Long working life. Excellent electrical insulation properties. Cures accelerated by heat. Chemically resistant. Low mixed viscosity. Serviceable from -80°F to +250°F. Two to one mix ratio by weight. Withstands impact. |
![]() |
EP37-3FLF Highly flexible, low viscosity, optically clear adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume. |
![]() |
EP37-3FLFAN Highly flexible, thermally conductive/electrically insulative epoxy system. Low viscosity. Cures readily at room temperature. Long working life. One to one mix ratio by weight or volume. Serviceable from 4K to +250°F. Good physical strength and chemical resistance. |
![]() |
EP37-3FLFAO Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting. |
![]() |
EP37-3FLFAOND Highly flexible, low viscosity adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume. |
![]() |
EP37-3FLSP Highly flexible. Low viscosity. Optically clear. Serviceable from 4K to +200°F. Superior dimensional stability. Long working life and low exotherm during curing. Ideal for large volume potting and casting. Excellent impact resistant. |
![]() |
EP37-3LV Clear, two component epoxy system has long pot life. Convenient one to one mix ratio. High bond strength. Superb chemical resistance properties. Used in bonding, sealing, potting and filament winding applications. Low viscosity compound. Exceptionally low exotherm. Cures rigid. Service operating temperature range from -60°F to +250°F. |
![]() |
EP38 Electrically insulative compound. Excellent flowability. High flexibility. Superior tensile and compressive strength. Cures quickly. Outstanding optical clarity. Protect against boiling water. Short tack free time. Low shrinkage upon cure. Easy to apply by roller, brush, spray equipment. Serviceable from -60°F to +250°F. |