EP77M-FMed Two Part Epoxy EP77M-FMed

Rapid room temperature curing silver filled electrically conductive adhesive. One to one mix ratio by weight or volume. Fixture time within 5-7 minutes even in small volumes. Exceptional low volume resistivity. Low outgassing. Superior bond strength to similar/dissimilar substrates. Serviceable from -60°F to +250°F.

EP79 Two Part Epoxy EP79

Cost effective alternative to silver filled epoxy with a silver coated nickel filler. Excellent conductivity and physical properties. Superior durability and thermal cycling capabilities. Cures readily at room temperature. Convenient one to one mix ratio weight or volume. Superb heat dissipation. Low linear shrinkage upon cure. Withstands 1,000 hours 85°C/85% RH. Serviceable from 4k to +275°F. Available in premixed and frozen syringes.

EP79FL Two Part Epoxy System EP79FL

Highly flexible, silver coated/nickel filled epoxy system. T-peel greater than 20 pli. Low volume resistivity. High bond strength to similar and dissimilar substrates. Resists exposure to thermal cycling. Serviceable from 4k to +275°F. One to one mix ratio by weight. Ambient temperature curing. 100% reactive. Withstands moisture, chemical exposure. Available in premixed and frozen syringes.

FL901S Epoxy Based Film FL901S

High performance, silver filled epoxy adhesive film system with outstanding electrical and thermal conductivity. Superior mechanical strength, convenient handling, good storage stability and fast cures at moderate temperatures. Specialty preforms are available. Serviceable from -100°F to +500°F.

MasterSil 151S Two Part Silicone System MasterSil 151S

Addition curing, two part silicone for use as an adhesive, sealant, coating or form-in-place gasketing material. Despite its silicone chemistry, it passes NASA low outgassing specifications. It is ideal for applications where low stress is required.

MasterSil 155 Two Part Silicone System MasterSil 155

Two part, graphite filled silicone adhesive. Convenient one to one mix ratio by weight. Volume resistivity 20-40 ohm-cm. Elongatio >300%. Serviceable from -85°F to +400°F.

Master Bond MasterSil 323S-LO Silicone System MasterSil 323S-LO

Addition curing, two part silicone for use as an adhesive, sealant, coating. Passes NASA low outgassing specifications. Serviceable from -80°F to +400°F. Electrically conductive with convenient processing.

MasterSil 705C One Part Silicone MasterSil 705C

Single component, electrically conductive, non-corrosive silicone compound. Carbon filled. Tack free time 3-7 minutes at ambient temperatures. Paste viscosity. Serviceable up to 400°F.

MastersSil 705S One Component Silicone MasterSil 705S

Silver filled, one-part, no-mix, non-corrosive silicone system. Shore A hardness 70. Cures at room temperatures when exposed to atmospheric moisture. Extremely low volume resistivity. Most effective when applied in thin sections.

MasterSil 973S-LO Two Part Silicone Compound MasterSil 973S-LO

Silver filled, two part, addition cured type silicone. Excellent electrical conductivity. Passes NASA low outgassing test requirements. Highly flexible. Service temperature range from -120°F to +400°F. Volume resistivit >0.004 ohm-cm.