EP46CA-1 Two Part Epoxy EP46CA-1

Serviceable from -100°F to +600°F. Tg>240°C. Oven curing. Used for structural bonding. High bond strength to similar/dissimilar surfaces. Withstands thermal cycling and chemical exposure. Electrical insulator. Long working life.

EP46HT Two Part Epoxy EP46HT

Heat resistant epoxy adhesive/sealant. Exhibits exceptional mechanical strength. Low viscosity system. Long pot life. Cures at elevated temperatures. Long term high temperature structural strength retention. Serviceable from -80°F to +500°F. Outstanding chemical resistance. Used in filament windings and with composite structures made from glass, polymide and graphic fiber.

EP46HT-1 Two Part Epoxy Compound EP46HT-1

Oven curing two part epoxy system. Resists from -100°F to +600°F. Tg of 230-240°C . Superb choice as matrix resin for fiber reinforced heat resistant composite structures. Exceptional strength properties. Robust chemical resistance. Long working life after mixing.

EP46HT-1AO Two Part Epoxy Compound EP46HT-1AO

Thermally conductive/electrically insulative heat resistant epoxy compound. Requires oven curing. Meets NASA low outgassing specifications. Meets MIL-STD-883J Section 3.5.2 for thermal stability. Excellent dimensional stability. Withstands 1,000 hours 85°C/85% RH. Serviceable from -100°F to +550°F. Tg 215-220°C.

EP46HT-1ND2 Two Part Epoxy System EP46HT-1ND-2

Heat resistant epoxy paste adhesive. Serviceable from -100°F to +600°F. Requires oven curing. Will not flow during processing. Superior electrical insulation and chemical resistant properties. Excellent mechanical strength.

EP46HT-2 Two Part Epoxy EP46HT-2

Serviceable from -100°F to +500°F. Tg 155-165°C. Superior durability. Heat curing, two component epoxy compound. Resists thermal cycling. Withstands 1,000 hours 85°C/85% RH. Good electrical insulator. Ability to protect against hostile chemical exposure.

EP46HT-2AO Black Two Part Epoxy EP46HT-2AO Black

Thermally conductive/electrically insulative. Passes NASA low outgassing tests. Serviceable from -100°F to +500°F. Tg 200-210°C. Remarkable dimensional stability. Impressive mechanical strength properties.

EP46HT-2Med Two Component Epoxy EP46HT-2Med

USP Class IV approved, heat resistant epoxy adhesive. Glass transition temperature in excess of 220°C. Withstands repeated exposure to autoclaving, radiation and chemical sterilants. High bond strength. Superior durability. Serviceable from -100°F to +500°F. Electrically insulative SUitable for potting.

EP46HT-2ND2 Two Part Epoxy Compound EP46HT-2ND2

Two part non-drip epoxy paste. Resists long term exposure from -100°F to +550°F. Superior peel strength. Protects against exposure to oils, fuels, hydrocarbons, acids, bases, solvents. Withstands thermal cycling and shock.

EP48TC Two Part Epoxy Adhesive EP48TC

Ultra low thermal resistance properties. Can be applied in bond lines as thin as 10-15 microns. Low CTE. Low shrinkage upon cure. Passes NASA low outgassing testing. Serviceable from -100°F to +300°F. Exceptional dimensional stability. Withstands 1,000 hours 85°C/85% RH.