EP4CL-80 One component, ultra low viscosity epoxy that offers thermal and electrical insulation and is optically clear. |
![]() |
EP4CL-80Med One component, ultra low viscosity epoxy that offers thermal and electrical insulation and is optically clear. |
![]() |
EP4EN-80 One component, low viscosity epoxy that offers thermal conductivity, electrical insulation and a filler material with ultra small particle sizes. This imparts high mechanical strength properties, outstanding dimensional stability and low shrinkage upon curing. |
![]() |
EP4G-80 Graphite filled epoxy that cures at 80°C. Good electrical and thermal conductivity. Passes NASA low outgassing certification. Can be used for bonding, sealing, coating. Service temperature range is -50°C to +175°C |
![]() |
EP4G-80Med Graphite filled epoxy that cures at 80°C. Good electrical and thermal conductivity. Passes ISO 10993-5 certification. Can be used for bonding, sealing, coating. Service temperature range is -50°C to +175°C |
![]() |
EP4NS-80 One component, optically clear, exceptionally low viscosity epoxy for bonding and sealing. Typically, curing is at 80°C for 2-4 hours, and for full optimization of properties, this should be followed by 110-125°C for 1-2 hours. Unlimited working life at room temperature. Excellent dimensional stability, low CTE and minimal shrinkage upon curing. |
![]() |
EP4S-80 One component, silver filled epoxy for bonding, sealing and coating. It is low in viscosity and flows smoothly and easily. Not premixed and frozen and has a working life of 8-12 hours; it will not cure until heated. Cure schedule is simple and straightforward, 60 to 90 minutes at 80°C. |
![]() |
EP4TC-80 One component epoxy for bonding, sealing and small encapsulation applications. High thermal conductivity and electrical insulation properties. Paste consistency epoxy featuring ultra fine particles filler material that allows application in very thin sections. High compressive strength, tensile modulus and dimensional stability. Serviceable from -50°C to +175°C. |
![]() |
EP4UF-80 One component, low viscosity epoxy primarily for underfill applications. Not premixed and frozen, with unlimited working life at room temperature. Cures at elevated temperatures with a minimum of 80°C. The service temperature range is -50°C to +150°C. |
![]() |
EP50-1.5 Rapid room temperature curing two component epoxy adhesive. Fixturing time of 5-8 minutes. Working life after mixing a 40 gram batch 2-3 minutes. One to one mix ratio by weight or volume. Solid tensile shear strength. Serviceable from 4K to +250°F. Available in different colors and viscosities. |